I was attempting to do two layers of glaze and applied wax over most up my sculpture, tape over another section and dipped. Well the glaze got everywhere and I still haven't been able to mop it all up. Its as if it seeped under the wax due to the very fine texture if the piece and became a stain. Is there anything I can do to rescue the piece? If there is some other coating that would go over the wax evenly?
All suggestions welcome:)