I've started experimenting with magma graces to create a faux volcanic surface. I'm using Mayco's dark magma glaze. results have been nice, but a bit too uniform and not as wild as some of the stuff I see online. If anyone has extensive experience with this technique I'd love to hear your recommendations. Have you tried mixing magma glazes? layering glazes? reglazing over and over, firing multiple times?