Hi, I noticed that sometimes after applying glaze, about 24 hours later, it sort of pulls away from the bisqueware.
Photos here: https://www.facebook.com/groups/maycomudroomsociety/permalink/1966264987085497/
I'm curious if it will still adhere to my piece in the cone 6 glaze firing that I plan to do soon? Or should I wash it all off and start over?
For context, these pieces are Laguna B mix (no grog), bisqued to cone 04 in a friend's electric kiln. I glazed the outside of each bowl by dipping 1 time, then brushed 2 coats of Mayco dark flux into the bottom of each bowl and then, after that was dry, poured Mayco dry glaze into the bowl and poured it out.
Thanks in advance for any help. Rachael