Hi everyone,
My kiln controller is broken and I can't see anything in the display. But I went ahead and fired it anyway after I guessed the temperature etc, crazy I know!!
Well the result was bubbles in my glaze. I was trying for 1260 cone 8 but I'm thinking it was programmed too high or maybe the ramps were too quick. Any help appreciated as I need to fire again soon. Yes I'm looking into getting fixed but it's a very busy time of year for me . I can't seem to post the photo, sorry.