Hello, I am digging a tunnel and have thousands upon thousands of pounds of clay. I intend to process it to make bricks. The problem I am facing is how do I process this quantity efficiently? There is a lot of sand and small rocks in it, water processing is slow for this quantity. I am unsure if this is the right place to be asking about this but I am at a loss. Any help is appreciated!
Large quantities of wild clay(water processing very slow)
in Clay and Glaze Chemistry
Posted
@Callie Beller Diesel I am looking to make bricks for a house. I'll have enough material to make several thousand bricks. My concern, based off lack of knowledge and use of clay is that I will fire the bricks and they will break apart. If I could use the clay as is that would be fantastic! I watched a video of Indian brick yard and their clay seemed processed in a way that wasn't explained. Im in western washington so sun drying wet clay isn't a problem. Also it's really fun to work with clay!