  1. Hello there, would really appreciate any help I can get! I have recently switched underglaze to the amaco velvet range due to their colour choice. I have also switched clear glazes but I think the new clear glaze (Cesco super gloss clear) is ruining the amaco colours when fired. My lovely dark olive green now looks like yellow / brown!! Is this because of the clear glaze? Or because of the firing? should I stick to the mayco clear glaze? Or maybe Amaco? See attached an example of the cesco clear glaze vs. the mayco clear glaze Please help!! i am meant to be launching products in 2 weeks time!
×
×