  1. @Mark C. I decided to bisque again to not risk losing the artwork and I’m glad I did too. I read what you wrote and decided to not take the risk.
  2. Hello! For clarification I’m using low fire earthenware clay 06 white clay EM330 from laguna clay I bisque fired yesterday and forgot to raise the hours on the timer for the kiln so it automatically shut off but I opened it this morning and the clay looks pretty vitrified… it does look delicate but is white not grey. I did notice a few had a few spots though! Do you think I should re-bisque? this order is time sensitive and needs to ship by Friday/tomorrow. Should I just glaze it? Do you think it’ll be okay?
×
×