I made a 20" high, 10" wide sculpture. I want it to stand slanted on a wooden base. The bottom is at an angle.
It weighs 8 lbs .
I made the edge that would be in contact with the base about 1" thick, and my idea is to insert 2 metal rods into this area that would attach it to the base.
It needs a very strong support.
Shall I drill the holes before firing, or at the bisque stage?
Any other ideas to attach it to the base?
Thanks