I have a constant chattering noise when I start up my 40 yr old Duncan EA 820-2. I have just replaced all the elements, the relay, the switch and someone else replaced the Kiln Sitter for me. I fired the kiln empty with 04 cone in the Kiln Sitter on the Hi Fire setting. All the elements glowed red and the Kiln Sitter turned off the Kiln after only 1 hour 15 min. The cone slumped as it should. I have 2 questions - 1. Is the chattering sound normal? if not - any idea as to what makes the chattering sound/how to fix it?
2. is my kiln firing too hot to quickly?
I will attach photos of the new parts added to the kiln. Thank you for your help.