Hi Friends hope you’re all well!
I am in desperate need for some help in getting my kiln to work again.
I have a 2 yr old L&L Equadpro 240v phase 1 kiln that I just changed the elements for the first time since buying it brand new 2 yrs ago
I did a quick glaze test firing on friday and it worked great (4.5hrs) Last night I loaded the kiln evenly and after 6 hrs it had only reached 360F . I re-started it before going to bed at 2am and at 8am it was only at 448F.
I have checked the wiring, the relays, the power, the fuses and thermocouples and all seem fine. I tried firing again and in 2 hrs it heated only about 80F
Any and all help is so incredibly appreciated! I am under a massive deadline and of course it had to do this to me now
Thank you all in advance!!