This summer I purchased an older kiln at an estate sale. I’ve attached photos of the controls, and the model number. I’ve tried to fire to cone 04 a few times for a test firing, but so far the kiln sitter shuts off around 5 hours, and the self supporting cone is barely bent.
The top dial, I’m assuming is the temp, and the second a timer.
does anyone have any suggestions on a firing schedule? So far I’ve tried 2nd knob ON — 1st knob 4 hours at low, the switched to medium, and then the sitter shuts off after about an hour at medium.
any advice would be so greatly appreciated!!!! Thank you!!
Bridget
Help firing an older Ceramichrome Autofire with Kiln Sitter
in Equipment Use and Repair
Posted
Thank you so much! Yes the weight was dropping early. I set the sitter time to 13 hours, but it dropped very early in the firing. Thank you so much for the link! Very helpful!!!