@Hulk The top of the handle has those little bumps. I'm not doing any holds or controlled cool. I fired this batch at cone 5 (typically I do cone 6) , at medium speed in a small studio kiln. Dont have exact dimensions but take about 8 hrs to reach temp then around 10 hrs to cool. I leave all the peep plugs plugged in, in both bisque and glaze firing. I do bisque fire to cone 04. Don't have a fan set up. When glaze firing, when it gets arond 500F I take out the peep plugs. I'm not expert, so if I'm wrong, please correct me! Also just want to add as an reminder, the other items in this firing, with the same clay but different glaze, turned out fine.