Hey Bill,
Thanks so much for your input. Yes it is a very large order, I have been making 100/day/7days a week, which is a lot. I will look into that link thank you for sending, in the meantime I have included a bit more information about this product below. Thank you!
Size ranges from 3"-9", closed form, made from 240 Standard white clay. Fired to cone 6 with a white glaze.