Any recommendation on propane setup for an updraft kiln?
I am trying to convert a 16 cu. ft gas kiln to propane using a 250 gallon tank. It uses 8 venturi burners. My first test using a 30 PSI adjustable regulator and 3/8 hose took me 8 hours to reach cone 06. The flame looked weak and yellowish. PSI was set around 8 and anything higher would shut the gas off. Is my regulator bad or not the correct for the BTU requirement?
Any feedback would be greatly appreciated. Thanks in advance.