  1. Has anyone experienced this? I ran a cone 5 firing load last night and just realized today that I selected the slow bisque setting instead of slow fire on my L&L Easy Fire. Still set to cone 5, just ran much slower. The temp read 2156 which is just a few degrees shy of a true Cone 5, but She’s still too hot to open. I was wondering/hoping if anyone had some insight into what to expect from this. While my kiln is easy to use, she doesn’t have any protective measures against someone with a foggy brain recovering from covid this past week.
×
×