I've been spending more and more time trying out new glazes, but I recently came into an issue while making test tiles. I've working with amaco brand velvet underglazes, and made up a pile of test tiles for the colors I currently have. I used the same procedure with all of them (bisque the tiles, two layers of underglaze, dry, two layers of clear, but on some of the tiles the color seems to have just vanished. I had the issue once before with a cup I had underglazed before bisque firing, but there the color faded during the second firing. I've attached a pictures of the fading tiles for reference.
Has anyone had these issue before? Am I screwing up the firing, or is it an issue with the glazes themselves? For reference, I'm firing in the 04-05 range.
Thanks in advance.