I'm in search for a good cone 5 firing schedule that create the least amount of defect,
we are firing a new skutt kiln KMT1027-3,
they use to firing on preprogram cone 5 schedule and are running into defects problems like pinhole and blisters.
I search around the wed and come up with this schedule,
step °F/hr / F Hold
1 200/180 60
2 200/1100 0
3 350/2053 5
4 100/2153 0
5 9999/2053 30
but still seeing pinhole on some glaze,
is it the glazing issues, or a firing issues?
I would love to hear from you guys.