Hi!
So I've tried several recipes of a low-fire clear dipping glazes and I'm getting generally the same results: cloudy/milky. Looking for solutions to this problem! Here are two recipes that I've used:
Silica 10
Neph Sye 20
EPK 10
Gerstley 30
Frit 3134and
Frit 3110 77
GB 6
EPK 7
Silica 10Would appreciate advice or another recipe. Thanks!