  1. Hi everyone, thanks for the answer. Yes, as mentioned, low fire shooting for the 06-04 range...Thanks for the input!
  2. Hi! So I've tried several recipes of a low-fire clear dipping glazes and I'm getting generally the same results: cloudy/milky. Looking for solutions to this problem! Here are two recipes that I've used: Silica 10 Neph Sye 20 EPK 10 Gerstley 30 Frit 3134 and Frit 3110 77 GB 6 EPK 7 Silica 10 Would appreciate advice or another recipe. Thanks!
×
×