  1. does the cone look like this? If it does it might have something to do with the old shimpo wheels
  2. Thanks. i checked ebay and the only pugmill part i could find was a nozzle. Now that I think about it I think I remember seeing a body for sale on there but it mustve sold
  3. Yea hell if its close enough ill do that. Whats the diameter and length? Thanks
  4. I found half of a nra-07 (pictured below) on offer up, i ended up paying $140 for it so i was willing to take that wager. Seeing how its 30something years old shimpo no longer makes replacement parts. Ive looked online but cant find much other than the “instructions” for it. Seeing as how it looks very similar to their more recent dual auger pugmills i was wondering is someone would do me the favor and take some measurements on theirs to see if using a newer models body would be feasible. Please dm me if you have an NVA-04 or NRA-04, thank you. Last resort will be me fabricating a body which i can probably do it since its kinda what I do for a living , but if possible want to avoid that headache.
  5. A year later but thought Id let everyone know how I fixed the issue in case anyone else ha the same problem. I took apart the switch and saw that the contacts were all pitted, i cleaned them up with a wire wheel on my dremel and tried it again. It worked. while I had the wheel on its side I noticed the wiring was starting to come apart( its a wheel from ‘71) so i replaced all wires since i already had the motor taken apart to clean and lubricate it. The rewiring has it running like a champ but I dont suggest you do it unless you know what youre doing. i love this wheel, it may be loud but it was made in an era were things were made to last, it will outlive me and im only in my 30s lol
  6. Hey, I have the same wheel and dealt with the same issue. Call laguna clay and ask them for PACIFICA SENSOR W/WAND + CORD, it was $23.75 when i bought it last year. Assuming we have the same pedal (cause I had the exact same issue) it should be a fairly easy fix. The only issue I had was i still havent really adjusted the pedal speed to were it wa originally, its not the end of the world it just annoys me sometimes. Does the inside of your pedal look like this picture? If so then ghats your fix. Ask the for the instructions, film yourself taking apart your pedal so u know exactly how it goes, dot lose anything (duh lol) . Hope this helps
×
×