    booth reacted to Rick Wise in Oxide washes on top of glazes! Oh my!   
    I post this as sort of a "public service" to other pottery semi-newbies like myself.  I somehow never got the message that you can easily paint oxide (and mason stain) washes on top of glazes for a lot of added color or design.  The videos below brought this to my attention and I am really excited about the results.  It has opened up some new avenues for me.  I defer to Richard McColl for a full description but it could not be easier:
    Just add some oxides (or mason stains), a little water, and maybe some gerstley borate as a flux -- and apply ON TOP of your glaze for great color and effects.  Goes on great with a brush.  Make it the consistency of ink.  Hard to screw up.
    Some examples are at the bottom and here are the videos:
     
     
     



×
×