  1. Hi everyone First time poster. I have a large kiln that is currently using spiral SiC elements. These are being degraded rapidly due to firing of PZT ceramics which are giving off lead and fluxing the silicon in the elements. The degradation only subtle but the spiral element runs into large problem because I end up with a conductive path between the positive and the negative terminal - shorting it all. Besides that the kiln is quite good. My question is: has anyone had any experience changing the element types in the kiln? I want to move from a spiral type to a U bar. I r
×
×