  1. I'm in need of stilts to suspend the interior of dome-shaped sculptures up to 4cm (so the rim/base doesn't touch the shelf surface). I've looked into heavy gauge nichrome wires, but I'm not sure if they'd be able to stand still during the high firing process, plus they are pretty difficult to cut. So I wonder if metal nails could be used as stilts. For example, the pointy part touches the sculptures, and the cap sticks into a flat body of clay, i.e., the base of the stilt. If so, what kind of nails can sustain in cone 10 firing? Thanks!
×
×