  1. Hello, I was wondering if anyone could help me, I have around 10 glaze fired tiles, they are all stoneware and I fired to 1200 with a 30 minute soak. 7 were glazed with textured brush on glazes and 3 were painted with a transparent glaze. For some reason when I took them all out of the kiln, all three transparent glazed ones and one beige tile appear to have several cracks in the back. The clay is a white stoneware clay, I placed them directly onto a batt washed kiln shelf and all three transparent tiles were on the top shelf. Not sure if this may be a coincidence. Please let me know if anyone has any suggestions as to how I can fix this issue?
×
×