So, I am a new high school art teacher who is in charge of the school's ceramics classes. When I was going through my classroom supplies, I learned that we have cone 6 clay, but all of our glaze is cone 06-04... SOS. What is the best way to use the supplies I have, when ordering new supplies at this time is not an option? I figured I could only fire the clay to cone 04, but then the work won't be as strong. Could I fire the clay to cone 6 as a "bisque" then follow it with a cone 04 glaze fire? Thank you in advance for any help offered!!!