UPDATE:
Here’s my piece I made in the end. I’m still finishing a vessel with a more mosaicy feel to it.
In the end I just had a go at it, but shrinkage has now happened on both pots pictured,, however, seen as this was just exploratory work for an art college project it’s okay!
Thank you again for everyone’s advice!