I have a number of glazes I have' not used in several years - will they be ok if I mix well and sieve them several times?
oldlady
hi, welcome to the forum. it might mix well if you made the glazes yourself. if they were bought as finished glazes, maybe not. the ingredients that are in bottled glazes do not blend well if they have dried out.
did you make the glazes?