  1. I have a Cress FX27P kiln. My kiln overheated during a glaze 06 fire.The kiln sitter cone was melted and did not work. I next did a bisque fire 04 and all seemed fine. I tired another glaze fire 06 it started up ok but when I went back an hour later to check it was not heating. The timers work but no heat. Did I burn out something?
×
×