  1. I bought a used paragon 10 sided TnF 23-3 kiln and just had the electrician here today to run wiring for it. I did a test to see if all of the elements worked and discovered that the two at the top and the two at the bottom glow bright red, YAY! However (this may be a newbie question), there seem to be about four in the middle that do not fire at all. Is this normal? What do I do next? It has a chip and some cracks in the brick in the lid that I can fix and I plan to set it on a stand and get a Orton VentMaster. Any other advice for me?
×
×