  1. New kiln user here. ...I’m trying to figure out if one of my relays are bad or if it’s my elements.  I can    Bisque To a 04 just fine. I did have a lose  connection to the relay. I fired again and it’s taking a long time. Any  suggestions?  It’s a  manual cress kiln. 

    1. neilestrick

      neilestrick

      Your best bet is to check the element resistance with a meter. If they're more than 10% off from new then they should be replaced. 

×
×