  1. Hi, I used the same one I’ve used for years this is why it’s baffled me so much. Never had problems with it before. I mixed the powder with water and when it fired it turned back into the powder I started with. I put a few thin layers on as it literally dries as soon as the brush hits the shelf. Then smoothed it over to create a flat surface.
  2. Thank you. It’s just baffling me as it’s never done this before.
  3. Hi I have recently applied Batt wash to my kiln shelves. This has been fired for the first time since reapplying it and the batt wash seems to have turned back to a powder and has fallen all over when lifting the kiln shelves out. This has never happened before and I am wondering if anyone can shed some light on why it’s turned to powder and if it is a problem. I mixed my own as usual from the batt wash powder I bought and applied a few coats.
×
×