5 hours ago, High Bridge Pottery said:
Does it have a review button so you can make sure the program is correct and rule out that being wrong?
I pressed the review button while the program was running but nothing happened…
-
9 hours ago, Babs said:
What controller do you have?
Whenyou stopped it and restarted it, what ramp did u notice it was displaying?
I am thinkinh like Bill, miutes instead of hours entered. Can you flick thro the ramps to see what u entered?
I have a KM controller. I wasn’t able to see what segment it was on - maybe there’s a way to do that while the program is running but I don’t know how.
-
1 hour ago, JRW said:
Hi All,
I have a new Skutt KM 1227 and am doing my first glaze firing (I’ve done one break-in firing and one bisque firing before).
I programmed the kiln to rise by 108f/hr to 195 degrees and hold for a few hours for a pre-heat (I was using shelves that were slightly damp from kiln wash).
For some reason the kiln just blew past that temperature and was at 216 before I caught it. I stopped the firing to let it cool a bit, then started it again, this time ramping to 200 degrees for the hold. Again, the kiln went up to 267 before I noticed it wasn’t holding.
the user manual says there will be an error code if the kiln stays more that 50 degrees hotter than the hold temperature for a given segment for at least 18 seconds. This situation met those criteria but there was no error displayed.
I’m just curious if anyone knows what might be causing this? I’m having trouble reaching Skutt and am on a deadline. I let the firing proceed but am worried the kiln won’t recognize the other holds I programmed. I didn’t program any holds in the bisque firing i did. Thanks!
Thanks, those are good ideas. I’m almost certain that I programmed the hold time correctly but it did occur to me that could be the issue. But twice?
The only other thing is that when the kiln was past the desired temp and I stopped the firing and restarted it, it was already above 200 degrees. (200 was the desired hold temp). So I assumed it would cool to 200 and then hold, but instead it just kept heating. I don’t know how the kiln algorithm handles a situation where it is supposed to be ramping up to a temperature but starts the firing program already above that temperature.
I will do a test on empty at a lower interval as you suggest. Thanks again!
-
Hi All,
I have a new Skutt KM 1227 and am doing my first glaze firing (I’ve done one break-in firing and one bisque firing before).
I programmed the kiln to rise by 108f/hr to 195 degrees and hold for a few hours for a pre-heat (I was using shelves that were slightly damp from kiln wash).
For some reason the kiln just blew past that temperature and was at 216 before I caught it. I stopped the firing to let it cool a bit, then started it again, this time ramping to 200 degrees for the hold. Again, the kiln went up to 267 before I noticed it wasn’t holding.
the user manual says there will be an error code if the kiln stays more that 50 degrees hotter than the hold temperature for a given segment for at least 18 seconds. This situation met those criteria but there was no error displayed.
I’m just curious if anyone knows what might be causing this? I’m having trouble reaching Skutt and am on a deadline. I let the firing proceed but am worried the kiln won’t recognize the other holds I programmed. I didn’t program any holds in the bisque firing i did. Thanks!
-
Thank you all for your input!
-
-
I just moved to a new studio and will be setting up a new Skutt 1227 kiln. I sold my envirovent 2 with my previous kiln, thinking I would get a different vent system. I was going to get the Bailey double vent system because it has a timer, which is a feature requested by some other members at my studio. (They have tried outlet timers for other vents and they haven’t worked for some reason so the timer is important).
https://www.baileypottery.com/m-405-009.html
This vent system requires leaving the top peephole open during firing and attaching a hose to the bottom two firebricks on the opposite side (holes are drilled). So, it’s kind of like a downdraft system, but not quite. I haven’t seen this design anywhere else and can’t find any reviews or comparisons, so I’m wondering if anyone here has any input. Is this comparable to other venting systems? Any red flags with this one?
Skutt kiln skipped a hold - no error code displayed
in Equipment Use and Repair
Posted
Thank you, that’s helpful!