  1. Awesome! Thank you. I guess it was confusing as to why the color was so much richer inside than out. I dipped them so The glaze seemed pretty think, then was beautiful inside (which presumably didn’t get as hot?) and didn’t quite get there on the inside. There’s so much to learn about glazing. Definitely in the trail and error (error error error) phase.
  2. Accidentally fired at cone 5 when I meant to fire at come 6 and the glazes didn’t do what I wanted (amaco iron luster under oatmeal - usually beautiful - is muddy and gross). Can I just refire it all at 6 or is it ruined? You can see that the inside is so different than the outside but it’s glazed the same? I’m so confused!
×
×