I am setting up a new kiln. Is there any change in the advice given in 2014 to use two layers of hardy board underneath the kiln?
neilestrick
No, it will work just fine. Put it on top of whatever your normal flooring is (wood?), and have it extend at least 12 inches beyond the kiln.