  1. Hi, For a bit of context I make pottery that I apply layers of slip to create a raised bumpy surface. When my work is in greenware stage the dots are easily knocked off, and although I can load my work with out knocking any off in my current studio situation Im not the one loading the kilns and I've been constantly getting pieces that have multiple dots missing. I was wondering if anyone knew of something that will help to keep attached pieces or slip trailing from being knocked off by people during loading. I was thinking maybe an organic hairspray or to coat the piece in wax
×
×