  1. Hello, Im a self taught potter. Im starting out wheel throwing. Im progressing well but as I attempt new forms I end up with my entire piece of clay needing to be recycled. What Im currently doing it sticking my clay with my other failed clay and wrapping it up in plastic. My plan is to reuse it but Im not sure the best way to dry the wet clay out without drying it to far. I only read about ways to recycle scraps. Any suggestions on how to recycle large pieces of failed clay?
×
×