  1. About 10 years ago, I took several ceramic classes and fell in love with the way Strontium Crystal Magic worked with other glazes. I attached a picture of Strontium Crystal Magic Warm with a spray of Water Color Green that I made in a community college class. Fast forward 10 years and I cannot get anything close to those results. The second picture shows the same glazes with a kiln controller set to a standard medium speed firing schedule to cone 5 with a 12 minute hold time. There are tons of nasty little pin-holes, and although I don't mind the color, it is nothing like I was expec
×
×