Hi All;
This weekend we did our first test firing for a new Cone Art Kiln. We used witness cones and fired to cone 6. We have a V6CF Bartlett Controller. When we opened the kiln my cone 5 witness cones were completely melted, the cone 6 and 7 cones were both completely layed over. The kiln controller had recorded a temperature of 2237 when it started to cool down. My cones are new as well. Any thoughts anyone? We are completely new to firing so want to figure this out before we do our first bisque firing.