  1. Thanks again everyone. Will think about the mixer and let you k ow. Have a great week.
  2. Thanks everyone. I’ve been following Chris Campbell for awhile now. She def has a lot of great information. I took a workshop from Karen Orsillo as well. Im going to try the slam method as well as look into the mixer. I appreciate what everyone has said.
  3. Hi, I have a lot of difficulty with wedging in large amounts of clay. I want to mix stains into 5 lb. increments of porcelain. Any suggestions on type of machine. Would A dough mixer or pug mill work. I’m not looking to spend a lot. It’s just for my home studio. Thanks, Liz
×
×