Michael Sorum
-
Posts
1 -
Joined
-
Last visited
Michael Sorum's Achievements
Newbie (1/3)
0
Reputation
Single Status Update
See all updates by Michael Sorum
-
making stone ware more plastic for the wheel? Mine is cracking, alot, when I try to stretch out a bowl, after I have rolled a texture on it? The stone ware was mixed, following a recipe, and I am doing fine with simple bowls but when I faceted one of my attempts and tried to stretch it i got alot of strecth cracks? My clay feels fairly soft and it was easy enough to center and pull. My sides were between 1/2" and 5/8", before I faceted with a cheese cutter. I cut slabs that are a little less than 1/8" thick. When I tried to strech it into the bowl shape with 5/16" sides, it cracks and splits? Any tricks?
-
Hi Michael!
May I suggest posting your question to "Clay and Glaze Chemistry" forum topic?
Several o' the regulars here might be able to help - could you include your recipe and ingredients, as well as process for mixing?
-
My recipe is at the studio, I will update and try to repost as you have suggested. Is there a how to article on how to post in the different forum topics? I am uneducated in these areas, sorry!
- Show next comments 3 more
-