  1. Thanks for the replies. The entire piece melted, after surviving a cone 04 bisque.. no other piece in the kiln melted. I don't think it was a mix up with clays because I only have the one white clay body in the studio.
  2. I fired several pieces made from Laguna Bmix clay WC401. They came out of the bisque firing of cone05 just fine, but when glazed and fired to cone 6 the pieces melted completely? Any idea why? The glazes were commercial cone 6 glazes. I've read you can fire to cone 6 with no problem.
×
×