Shelly M reacted to Marcia Selsor for a gallery image, cone 6 Faux Celedon
Selsor Faux Celedon ^6 Oxidation
Whiting 18.5
Neph Syen 25.8
EPK 18.8
Silica 31.1
Gerstley B 4.6
98.8
Copper carb 0.3
Mason #6600 Black 0.02