Report 127919E4-2DCA-4B5E-9553-CCE410D183CF.jpeg in Browse Member Galleries 1 Posted October 17, 2022 Refired in electric to 04 after cone 03 reduction cooled glaze fire. I was trying to get rid of some pinholes. The lustrous surface is not a photography artifact, this pot is beautifully metallic. Unexpected. Hulk 1
127919E4-2DCA-4B5E-9553-CCE410D183CF.jpeg
in Browse Member Galleries
1Posted
Refired in electric to 04 after cone 03 reduction cooled glaze fire. I was trying to get rid of some pinholes. The lustrous surface is not a photography artifact, this pot is beautifully metallic. Unexpected.