Anchorage Wild Clay
Local clay from my area. Porous at cone 04, vitreous at 03, slumping and bloating at 02. Glazed on the inside, the exterior is bare clay with terra sigillata (made from the same clay). The darker pieces are reduction cooled. Blacks are from reduced iron, not carbon or smoke.
- Album created by Kelly in AK
- Updated
- 13 images
- 1 image comment
- 13 images
- 1 image comment
-
Cone 6 Soda Fired
Mostly white stoneware (BC6 from Clay Art Center in Tacoma) with a Helmer kaolin slip (50 Helmer/50 neph sy).