Status Updates posted by cam
-
I am wondering about glazing in a cold garage ( 27^) The bisque is cold, the glazes are cold. Does this affect the outcome? or is it of no concern
- Show previous comments 2 more
-
It'll be uncomfortable for you, but your pots won't care. Don't let the glaze bucket freeze though. It'll hard pan like nothing else I've ever seen.
-
You should probably heat the pottery up very slow. I remember a potter friend I had many moons ago. He had a studio the size of an airplane hanger. Anyway, he had a ceremonial platter he had to fire, but it was below freezing and he was in a hurry. He could have waited, but he didn't. The plate blew into a million pieces.
-
oh dear!
thnx guys...we'll see tomorrow