jevpots got a reaction from Hulk in Laser Gas Kiln Help
I find how you arrange the kiln shelves affects the heat circulation. Slightly overlapping bottom to top on the burner side and keeping the backs close to the back wall send to help me. I also have the model with the turbo fan which adds an extra dimension to circulation. I put thermocouples in the top and bottom bung holes to give me extra feedback too.