  1. Thanks Marcia. I add mason stains to southern ice porcelain. Each piece is rolled out by hand twice so it's transparent and also cut twice. They are fired to cone 9 oxidation. I insert them into styrofoam that has been hollowed out. I add flameless tealights inside.

×
×