  1. Thanks! Good points- iron or salts & maybe they would burn off In next firing. I have a few pieces like this, I can test it & see what happens.
  2. I’m using plain terra sig made with xx saggar on Laguna 80 red clay. I bisqued and remained waxy and white. Perfect. then I added Psuedo Celedon glaze to the interior of the cylinder. Some dripped so I wiped off the whole pot with a wet clean sponge. When it dried, the white Terra Sig started turning bright yellow. Marker yellow. Won’t wash off... Any idea why this would happen?
×
×