DFerragamo got a reaction from Tatyana for a gallery image, The Bird Caller
Stoneware with commercial glaze. Fired to cone 6 in oxidation.
I make a series of these Bird Caller figures. Each is slightly different, but all with the same theme, girls with birds on their arms.
-
DFerragamo got a reaction from dolly for a gallery image, Bear Spirit Guide
Hand built stoneware, 11 inches, cone 5, oxidation.
I make my animal spirit guides with many different kinds of animals.