  1. has anyone used patch a tatch? on greenware?

    1. LeeU

      LeeU

      Am not familiar with it. I try not to repair anything I can remake but have used Spooze (do a search if interested-there is a recipe for it) with great success on greenware that I just had to keep going with, and it always fired great...no sign of a crack or break. 

×
×